Stainless Steel Foil
Crucible offers two grades of stainless steel foil wrap for use in preventing surface decarburization of tools or other metal products during heat treatment in furnaces not equipped with atmosphere controls. The selection of foil type is determinded by the operating temperature as indicated below:

Max.
Temp.
Grade
Thickness
inch
Width
inch
Length
ft.

2000F
321
0.002
24
50, 100, 200
0.003
24
50, 100
2240F
309
0.002
24
50, 100

Crucible Stainless Steel Foils are shipped from the Milwaukee Service Center in convenient cardboard dispenser cartons.