STAINLESS TOOL STEELS CHEMISTRIES & PROPERTIES
|
|
AISI |
GRADE NAME |
C |
Cr |
V |
Mo |
OTHER |
WEAR
RESISTANCE
|
TOUGHNESS
|
CORROSION
RESISTANCE
|
|
|
416 |
416 R |
0.12 |
12.50 |
|
0.40 |
0.13 S |
|
|
|
|
17Cr-4Ni MOD |
CRUCIBLE 174 SXR |
0.02 |
15.00 |
|
0.20 |
3.5 Cu, 4.75 Ni |
|
|
|
|
414 MOD |
MAXEL 2000 |
0.03 |
12.50 |
|
0.30 |
2.75 Ni, 0.12 S |
|
|
|
|
17Cr-4Ni MOD |
CSM 21 |
0.02 |
15.00 |
|
0.20 |
3.50 Cu, 4.75 Ni |
|
|
|
|
420 PREM |
CSM 420 XL |
0.38 |
13.60 |
0.30 |
|
|
|
|
|
|
440C |
CRUCIBLE 440C |
1.00 |
17.50 |
|
0.50 |
|
|
|
|
|
440C MOD |
154 CM |
1.05 |
14.00 |
|
4.00 |
|
|
|
|
|
440C MOD +V |
CPM S60V (440V) |
2.15 |
17.00 |
5.50 |
0.40 |
|
|
|
|
|
420 MOD +V |
CPM S90V (420V) |
2.35 |
14.00 |
9.00 |
1.00 |
|
|
|
|
|
|